... ... @@ -1,7 +1,60 @@
1 1  The Multi-Light Workstation support several laser marking methods. Choosing the right on depends on the material, the visual/functional goal, and your process constraints (cycle time, depth, readability).
2 +
2 2  
3 3  = Engraving =
4 4  
5 -What it is: Material removal to create a permanent recess.
6 -Best for: Metals (steel, stainless steel, aluminum), some hard plastics.
6 +**What it is**: Material removal to create a permanent recess.
7 +**Best for**: Metals (steel, stainless steel, aluminum), some hard plastics.
8 +**Result**: Matte, tactile mark with depth; excellent durability.
9 +**Notes**:
10 +
11 +* Depth increases with **higher energy **and/or **multiple passes**.
12 +* Use **fills (hatching)** rather than outlines for solid areas.
13 +* Manage heat to avoid warping thin parts (optimize speed, spacing, repetitions).
14 +
15 +
16 +
17 += Annealing =
18 +
19 +**What it is**: **Oxide-layer color change** on steel/stainless steel without material removal.
20 +**Best for**: Stainless steel, some alloy steels.
21 +**Results**: Dark (often black to brown) high-contrast mark; **no tactile depth**.
22 +**Notes**:
23 +
24 +* Keep **energy density moderate**; the mark comes from controlled heating, not ablation.
25 +* Great for applications where **surface integrity** must remain untouched. (e.g., medical).
26 +
27 +
28 +
29 += Carbonizing =
30 +
31 +**What it is**: Local heating on certain **plastics **creating carbonized dark marks.
32 +**Best for**: Light plastics where high contrast is needed.
33 +**Results**: Darkened characters/graphics with good readability
34 +**Notes**:
35 +
36 +* Avoid excessive heat - can cause melt, bulge, or halo.
37 +* Typically **lower speed** + **controlled power** to "bloom" contrast without charring.
38 +
39 +
40 +
41 += Foaming =
42 +
43 +**What it is**: Heat induces **gas bubbles** under the plastic surface, creating a **raised**, **lighter **mark.
44 +**Best for**: Dark plastics where light marks are desired.
45 +**Results**: Light, slightly raised mark; good for UI panels, housings.
46 +**Notes**:
47 +
48 +* Tune energy so bubbles form uniformly - over-energy can collapse structure.
49 +* Usually faster speeds with moderate power work well.
50 +
51 +
52 +
53 += Layer Removal =
54 +
55 +**What it is**: Selective ablation 
56 +**Best for**:
57 +**Results**:
58 +**Notes**:
59 +
7 7