Changes for page Marking Methods

Last modified by jadomatis on 2026/09/07 11:07

From version 1.13
edited by jadomatis
on 2025/09/30 12:12
Change comment: There is no comment for this version
To version 2.1
edited by jadomatis
on 2025/09/30 12:45
Change comment: There is no comment for this version

Summary

Details

Page properties
Content
... ... @@ -52,9 +52,51 @@
52 52  
53 53  = Layer Removal =
54 54  
55 -**What it is**: **Selective ablation **of top coatin
56 -**Best for**:
57 -**Results**:
55 +**What it is**: **Selective ablation **of top coatings (paint, anodizing, powder coat) to reveal the base.
56 +**Best for**: Anodized aluminum, painted/coated metals, laminates.
57 +**Results**: High-contrast graphics/logos with crisp edges; fast cycles on thin coatings.
58 58  **Notes**:
59 59  
60 -
60 +* Use j**ust enough energy **to remove the **coating only**.
61 +* Fine hatching and one or two passes often suffice; avoid attacking the substrate.
62 +
63 +
64 +
65 += Foil Marking =
66 +
67 +**What it is**: Marking through or onto **films/foils** (e.g., label stock, laminates)
68 +**Best for**: Decorative or functional labels; layered materials.
69 +**Results**: Clean symbols/text; can combine with kiss-cutting depending on stack-up.
70 +**Notes**:
71 +
72 +* Verify foil behavior (melt/edge quality); adjust speed and hatch for **clean edges**.
73 +* Ensure reliable **extraction **- thin films can produce sticky aerosols.
74 +
75 +
76 +
77 += Choosing a Method - Quick Guidance =
78 +
79 +|=Goal/Material|=Recommended method(s)
80 +|Deep, durable on metal|Engraving (multi-pass fill)
81 +|High contrast on stainless, removal|Annealing
82 +|Dark text on light plastic|Carbonizing
83 +|Light text on dark plastic|Foaming
84 +|Logo on anodized aluminum/paint |Layer Removal
85 +|Labels/multilayer foils |Foil Marking
86 +
87 +
88 +
89 += Good Practices Across All Methods =
90 +
91 +* **Focus first**: Z-axis focus is the single biggest quality lever.
92 +* **Start conservative**: Prove the look with lower energy, then optimize cycle time.
93 +* **Use fills wisely**: Hatch angle and line spacing control contrast, smoothness, and time.
94 +* **Control heat**: Balance power, speed, repetitions to avoid discoloration, melt, or halos.
95 +* **Extract fumes**: Protect optics and improve consistency - especially for plastics and coatings.
96 +* **Document presents**: Save verified parameters sets per material/finish for repeatability.
97 +
98 +
99 +
100 += Summary =
101 +
102 +Multi-Light can produce **deep engravings**, **oxide-layer anneals**, **carbonized or foamed plastic marks**, **clean coating removals**, and **foil marks**. Match the method to the material and end-use requirement, dial in parameters methodically, and rely on extraction and focus discipline for consistent, high-quality results.