Changes for page Marking Methods
Last modified by jadomatis on 2026/09/07 11:07
Summary
-
Page properties (1 modified, 0 added, 0 removed)
Details
- Page properties
-
- Content
-
... ... @@ -16,45 +16,10 @@ 16 16 17 17 = Annealing = 18 18 19 -**What it is**: **Oxide-layer color change** on steel/stainless steel without material removal. 20 -**Best for**: Stainless steel, some alloy steels. 21 -**Results**: Dark (often black to brown) high-contrast mark; **no tactile depth**. 22 -**Notes**: 19 +What it is: Oxide-layer color change on steel/stainless steel without material rem 20 +Best for: 21 +Results: 22 +Notes: 23 + 23 23 24 -* Keep **energy density moderate**; the mark comes from controlled heating, not ablation. 25 -* Great for applications where **surface integrity** must remain untouched. (e.g., medical). 26 - 27 - 28 - 29 -= Carbonizing = 30 - 31 -**What it is**: Local heating on certain **plastics **creating **carbonized **dark marks. 32 -**Best for**: Light plastics where high contrast is needed. 33 -**Results**: Darkened characters/graphics with good readability 34 -**Notes**: 35 - 36 -* Avoid excessive heat - can cause melt, bulge, or halo. 37 -* Typically **lower speed** + **controlled power** to "bloom" contrast without charring. 38 - 39 - 40 - 41 -= Foaming = 42 - 43 -**What it is**: Heat induces **gas bubbles** under the plastic surface, creating a **raised**, **lighter **mark. 44 -**Best for**: Dark plastics where light marks are desired. 45 -**Results**: Light, slightly raised mark; good for UI panels, housings. 46 -**Notes**: 47 - 48 -* Tune energy so bubbles form **uniformly **- over-energy can collapse structure. 49 -* Usually **faster speeds** with **moderate power** work well. 50 - 51 - 52 - 53 -= Layer Removal = 54 - 55 -**What it is**: **Selective ablation **of top coatin 56 -**Best for**: 57 -**Results**: 58 -**Notes**: 59 - 60 60