Changes for page Marking Methods

Last modified by jadomatis on 2026/09/07 11:07

From version 1.11
edited by jadomatis
on 2025/09/30 12:07
Change comment: There is no comment for this version
To version 1.9
edited by jadomatis
on 2025/09/30 11:27
Change comment: There is no comment for this version

Summary

Details

Page properties
Content
... ... @@ -26,29 +26,6 @@
26 26  
27 27  
28 28  
29 -= Carbonizing =
30 30  
31 -**What it is**: Local heating on certain plastics creating carbonized dark marks.
32 -**Best for**: Light plastics where high contrast is needed.
33 -**Results**: Darkened characters/graphics with good readability
34 -**Notes**:
35 35  
36 -* Avoid excessive heat - can cause melt, bulge, or halo.
37 -* Typically **lower speed** + **controlled power** to "bloom" contrast without charring.
38 -
39 -
40 -
41 -= Foaming =
42 -
43 -**What it is**: Heat induces gas bubbles under the plastic surface, creating a raised, lighter mark.
44 -**Best for**: Dark plastics where light marks are desired.
45 -**Results**: Light, slightly raised mark; good for UI panels, housings.
46 -**Notes**:
47 -
48 -* Tune energy so bubbles form uniformly - over-energy can collapse structure.
49 -* Usually faster speeds with moderate power work well.
50 -
51 -
52 -
53 -
54 54