Wiki source code of Marking Methods
Show last authors
| author | version | line-number | content |
|---|---|---|---|
| 1 | The Multi-Light, Multi-Light PLUS, Auto-Light, and High-Light workstations support several laser marking methods. Choosing the right on depends on the material, the visual/functional goal, and your process constraints (cycle time, depth, readability). | ||
| 2 | |||
| 3 | = Engraving = | ||
| 4 | |||
| 5 | //Material removal to create a permanent recess.// | ||
| 6 | **Best for**: Metals (steel, stainless steel, aluminum), some hard plastics. | ||
| 7 | **Result**: Matte, tactile mark with depth; excellent durability. | ||
| 8 | **Notes**: | ||
| 9 | |||
| 10 | * Depth increases with **higher energy **and/or **multiple passes**. | ||
| 11 | * Use **fills (hatching)** rather than outlines for solid areas. | ||
| 12 | * Manage heat to avoid warping thin parts (optimize speed, spacing, repetitions). | ||
| 13 | |||
| 14 | |||
| 15 | |||
| 16 | = Annealing = | ||
| 17 | |||
| 18 | //**Oxide-layer color change** on steel/stainless steel __without material removal__.//[[image:1759236605060-439.png||data-xwiki-image-style-alignment="end" height="117" width="115"]] | ||
| 19 | **Best for**: Stainless steel, some alloy steels. | ||
| 20 | **Results**: Dark (often black to brown) high-contrast mark; **no tactile depth**. | ||
| 21 | **Notes**: | ||
| 22 | |||
| 23 | * Keep **energy density moderate**; the mark comes from controlled heating, not ablation. | ||
| 24 | * Great for applications where **surface integrity** must remain untouched. (e.g., medical). | ||
| 25 | |||
| 26 | |||
| 27 | |||
| 28 | = Carbonizing = | ||
| 29 | |||
| 30 | //Local heating on certain **plastics **creating **carbonized **dark marks.// | ||
| 31 | [[image:1759236564557-618.png||data-xwiki-image-style-alignment="end" height="67" width="235"]]**Best for**: Light plastics where high contrast is needed. | ||
| 32 | **Results**: Darkened characters/graphics with good readability | ||
| 33 | **Notes**: | ||
| 34 | |||
| 35 | * Avoid excessive heat - can cause melt, bulge, or halo. | ||
| 36 | * Typically **lower speed** + **controlled power** to "bloom" contrast without charring. | ||
| 37 | |||
| 38 | |||
| 39 | |||
| 40 | = Foaming = | ||
| 41 | |||
| 42 | //Heat induces **gas bubbles** under the plastic surface, creating a **raised**, **lighter **mark.//[[image:1759236739160-895.png||data-xwiki-image-style-alignment="end" height="133" width="258"]] | ||
| 43 | **Best for**: Dark plastics where light marks are desired. | ||
| 44 | **Results**: Light, slightly raised mark; good for UI panels, housings. | ||
| 45 | **Notes**: | ||
| 46 | |||
| 47 | * Tune energy so bubbles form **uniformly **- over-energy can collapse structure. | ||
| 48 | * Usually **faster speeds** with **moderate power** work well. | ||
| 49 | |||
| 50 | |||
| 51 | |||
| 52 | = Layer Removal = | ||
| 53 | |||
| 54 | //**Selective ablation **of top coatings (paint, anodizing, powder coat) to reveal the base.// | ||
| 55 | [[image:1759236649259-613.png||data-xwiki-image-style-alignment="end" height="113" width="200"]]**Best for**: Anodized aluminum, painted/coated metals, laminates. | ||
| 56 | **Results**: High-contrast graphics/logos with crisp edges; fast cycles on thin coatings. | ||
| 57 | **Notes**: | ||
| 58 | |||
| 59 | * Use j**ust enough energy **to remove the **coating only**. | ||
| 60 | * Fine hatching and one or two passes often suffice; avoid attacking the substrate. | ||
| 61 | |||
| 62 | |||
| 63 | |||
| 64 | = Foil Marking = | ||
| 65 | |||
| 66 | //Marking through or onto **films/foils** (e.g., label stock, laminates).//[[image:1759236782973-114.png||data-xwiki-image-style-alignment="end" height="159" width="221"]] | ||
| 67 | **Best for**: Decorative or functional labels; layered materials. | ||
| 68 | **Results**: Clean symbols/text; can combine with kiss-cutting depending on stack-up. | ||
| 69 | **Notes**: | ||
| 70 | |||
| 71 | * Verify foil behavior (melt/edge quality); adjust speed and hatch for **clean edges**. | ||
| 72 | * Ensure reliable **extraction **- thin films can produce sticky aerosols. | ||
| 73 | |||
| 74 | |||
| 75 | |||
| 76 | = Choosing a Method - Quick Guidance = | ||
| 77 | |||
| 78 | |=Goal/Material|=Recommended method(s) | ||
| 79 | |Deep, durable on metal|Engraving (multi-pass fill) | ||
| 80 | |High contrast on stainless, removal|Annealing | ||
| 81 | |Dark text on light plastic|Carbonizing | ||
| 82 | |Light text on dark plastic|Foaming | ||
| 83 | |Logo on anodized aluminum/paint |Layer Removal | ||
| 84 | |Labels/multilayer foils |Foil Marking | ||
| 85 | |||
| 86 | |||
| 87 | |||
| 88 | = Method Applicability = | ||
| 89 | |||
| 90 | (% class="table-condensed table-striped" %) | ||
| 91 | |=Marking method|=(% style="width: 141px;" %)Multi-Light|=(% style="width: 136px;" %)Multi-Light PLUS|=(% style="width: 136px;" %)Auto-Light|=(% style="width: 126px;" %)High-Light|=(% style="width: 441px;" %)Important difference | ||
| 92 | |Engraving|(% style="width:141px" %)Supported|(% style="width:136px" %)Supported|(% style="width:136px" %)Supported|(% style="width:126px" %)Supported|(% style="width:441px" %)Achievable depth and heat input depend on power, pulse behavior, lens, and laser source. High-Light UV and UKP results must be qualified separately from fiber engraving. | ||
| 93 | |Annealing|(% style="width:141px" %)Supported on suitable steel and titanium|(% style="width:136px" %)Same process|(% style="width:136px" %)Same process|(% style="width:126px" %)Source-depended|(% style="width:441px" %)MOPA pulse control can provide more adjustment of color and heat input. Do not assume fiber parameter will work with UV and UKP sources | ||
| 94 | |Carbonization|(% style="width:141px" %)Supported on compatible light plastics|(% style="width:136px" %)Same process|(% style="width:136px" %)Same process|(% style="width:126px" %)Source-depended|(% style="width:441px" %)Polymer absorption changes with wavelength. Compatibility must be verified separately for fiber, UV, and UKP configurations. | ||
| 95 | |Foaming|(% style="width:141px" %)Supported on compatible dark plastics|(% style="width:136px" %)Same process|(% style="width:136px" %)Same process|(% style="width:126px" %)Source-depended|(% style="width:441px" %)Plastic grade, additives, colorant, wavelength, and pulse duration a | ||
| 96 | |Layer removal|(% style="width:141px" %)Supported|(% style="width:136px" %)Same process with greater workpiece capacity|(% style="width:136px" %)Same process in the integrated host machine|(% style="width:126px" %)Source-depended|(% style="width:441px" %) | ||
| 97 | |Foil application|(% style="width:141px" %)Supported|(% style="width:136px" %)Supported|(% style="width:136px" %)Supported|(% style="width:126px" %)Supported with a suitable source|(% style="width:441px" %) | ||
| 98 | |Ablation foil marking and cutting|(% style="width:141px" %)Accessory-depended|(% style="width:136px" %)Accessory-depended|(% style="width:136px" %)Accessory-depended|(% style="width:126px" %)Accessory-depended|(% style="width:441px" %) | ||
| 99 | |||
| 100 | |||
| 101 | |||
| 102 | |||
| 103 | = Good Practices Across All Methods = | ||
| 104 | |||
| 105 | * **Focus first**: Z-axis focus is the single biggest quality lever. | ||
| 106 | * **Start conservative**: Prove the look with lower energy, then optimize cycle time. | ||
| 107 | * **Use fills wisely**: Hatch angle and line spacing control contrast, smoothness, and time. | ||
| 108 | * **Control heat**: Balance power, speed, repetitions to avoid discoloration, melt, or halos. | ||
| 109 | * **Extract fumes**: Protect optics and improve consistency - especially for plastics and coatings. | ||
| 110 | * **Parameter presets**: Save verified parameter sets per material/finish for easy reuse. | ||
| 111 | |||
| 112 | |||
| 113 | |||
| 114 | = Summary = | ||
| 115 | |||
| 116 | Both Multi-Light and Multi-Light PLUS can produce **deep engravings**, **oxide-layer anneals**, **carbonized or foamed plastic marks**, **clean coating removals**, and **foil marks**. Match the method to the material and end-use requirement, dial in parameters methodically, and rely on extraction and focus discipline for consistent, high-quality results. |